Ceramic · Thermal Conductivity
Thermal Conductivity of Soda-Lime Glass
The thermal conductivity of Soda-Lime Glass is approximately 1 W/(m·K). How readily heat flows — drives conduction in thermal analysis.
Thermal Conductivity of Soda-Lime Glass
1 W/(m·K)
Ranked #36 of 53 materials by thermal conductivity
Compared to nearby materials
| Concrete | 1.7 W/(m·K) |
| Fused Silica | 1.4 W/(m·K) |
| Borosilicate Glass | 1.2 W/(m·K) |
| Soda-Lime Glass | 1 W/(m·K) |
| HDPE | 0.48 W/(m·K) |
| Fiberglass (GFRP) | 0.3 W/(m·K) |
| PETG | 0.29 W/(m·K) |
Related products
Solver Method Recommendation Report
$4Describe your problem; get the recommended method and settings.
Reports & IntelligenceView →
Live Monthly Office Hours
$9A live Q&A session with a simulation specialist.
Courses & TrainingView →
Verified Researcher Badge
$19/yrAn annual verified-researcher badge on your public profile.
Annual MembershipsView →
Data Export Pack
$2Unlock bulk CSV/HDF5 export for a project's full result set.
Compute & CreditsView →
Multi-Physics Solver Session
$12A coupled multi-physics solve linking fluid, thermal, and structural nodes.
Premium ToolsView →
Biology Simulation Kit
$19Population dynamics, reaction networks, and cellular models.
Bundles & KitsView →